🇵🇱 ARCELORMITTAL POLAND S.A. PL
Materials & polymersPetrochemistry & fuels
ARCELORMITTAL POLAND S.A. is a laboratory accredited by PCA under number AB 1449 (Dąbrowa Górnicza, Poland). Its accreditation scope covers 16 test methods in the following areas: Materials & polymers, Petrochemistry & fuels. Test objects include: Steel products, Steel, Ferroalloys, Solid fuels: coke. Most frequently used techniques: High-temperature combustion with IR detection, Gravimetric method, Brinell method.
At a glance
- Accreditation number: PCA AB 1449
- Methods in scope: 16
- Types of test objects: 7
- Techniques used: 7
- City: Dąbrowa Górnicza, Poland
- Accreditation number
- AB 1449
- Accreditation body
- PCA
- Address
- LABORATORIA BADAŃ JAKOŚCIOWYCH, Al. J. Piłsudskiego 92, 41-308 Dąbrowa Górnicza
- City
- Dąbrowa Górnicza, Poland
What this laboratory tests (7)
- Steel products — 8 methods
- Steel — 3 methods
- Ferroalloys — 1 method
- Solid fuels: coke — 1 method
- Solid fuels: hard coal, Anthracite, carburiser — 1 method
- Solid fuels: hard coal, coke, Anthracite, carburiser, Raw materials of the metallurgical process: - iron ores and mineral aggregates, Semi-finished products of the metallurgical process, Dusts, sludges, mill scale, dross, slags from the metallurgical process — 1 method
- Steel, cast iron, pig iron — 1 method
Analytical techniques used (7)
- High-temperature combustion with IR detection — 3 methods
- Gravimetric method — 2 methods
- Brinell method — 1 method
- High-temperature extraction with IR detection — 1 method
- High-temperature extraction with TC detection — 1 method
- Metallographic method — 1 method
- Spark excitation atomic emission spectrometry — 1 method
Laboratory sections (3)
- Spectrometric and Chemical Laboratory; Al. J. Piłsudskiego 92, 41-308 Dąbrowa Górnicza — 8 methods
- Mechanical Testing Laboratory Dąbrowa Górnicza; Al. J. Piłsudskiego 92, 41-308 Dąbrowa Górnicza — 6 methods
- Mechanical Testing Laboratory - Kraków — 2 methods
Laboratory locations
- Laboratorium Spektrometryczne i Chemiczne — Al. J. Piłsudskiego 92, 41-308 Dąbrowa Górnicza
- Laboratorium Badań Mechanicznych Dąbrowa Górnicza — Al. J. Piłsudskiego 92, 41-308 Dąbrowa Górnicza
- Laboratorium Badań Mechanicznych - Kraków — ul. T. Sendzimira 1, 31-752 Kraków
- Laboratorium Badań Mechanicznych Dąbrowa Górnicza; Al. J. Piłsudskiego 92, 41-308 Dąbrowa Górnicza —
- Laboratorium Spektrometryczne i Chemiczne; Al. J. Piłsudskiego 92, 41-308 Dąbrowa Górnicza —
Accreditation scope — test methods (16)
| No. | Test object | Methodology / Parameters | Technique | Reference document | |
|---|---|---|---|---|---|
| Spectrometric and Chemical Laboratory; Al. J. Piłsudskiego 92, 41-308 Dąbrowa Górnicza | |||||
| 1 | Steel, cast iron, pig iron | Content of: C,S carbon - (0,01 - 5,00) % sulfur - (0,001 - 0,400) % | High-temperature combustion with IR detection | PB/S9.2/L.202 wydanie 3 z dnia 31.03.2022 | |
| 2 | Ferroalloys | Content of: C,S carbon - (0,01 – 10,00) % sulfur - (0,002 - 0,150) % | High-temperature combustion with IR detection | PB/S9.2/L.202 wydanie 3 z dnia 31.03.2022 | |
| 3 | Solid fuels: hard coal, coke, Anthracite, carburiser, Raw materials of the metallurgical process: - iron ores and mineral aggregates, Semi-finished products of the metallurgical process, Dusts, sludges, mill scale, dross, slags from the metallurgical process | Content of: C,S carbon - (0,01 - 99,99) % sulfur - (0,003 – 7,40) % | High-temperature combustion with IR detection | PB/S9.2/L.203 wydanie 5 z dnia 20.05.2025 | |
| 4 | Steel | Content of: C, Mn, Si, P, S, Cu, Cr, Ni, Al, Mo, V, Nb, Sn, As, Ti, Sb, N, B, Pb, W, Co, Zr carbon (0,004 - 1,600) % manganese (0,006 – 2,200) % silicon (0,001 – 0,900) % phosphorus (0,001 – 0,065) % sulfur (0,002 - 0,070) % copper (0,006 - 0,600) % chromium (0,003 - 1,200) % nickel (0,002 - 0,800) % aluminium (0,001 - 0,110) % molybdenum (0,001 - 0,450) % vanadium (0,001 - 0,200) % niobium (0,002 - 0,140) % tin (0,001 - 0,180) % arsenic (0,001 - 0,090) % titanium (0,001 - 0,180) % antimony (0,001 - 0,030) % nitrogen (0,0018 - 0,0170) % boron (0,0003 - 0,0130) % lead (0,001 - 0,040) % tungsten (0,003 - 1,500) % cobalt (0,001 - 0,060) % zirconium (0,001 - 0,060) % | Spark excitation atomic emission spectrometry | PB/S9.2/L.228 wydanie 4 z dnia 10.03.2026 | |
| 5 | Steel | Oxygen content Range (0,0003 – 0,0125) % |
High-temperature extraction with IR detection | PB/S9.2/L.226 wydanie 4 z dnia 10.04.2024 | |
| 6 | Steel | Nitrogen content Range (0,0003 – 0,0450) % |
High-temperature extraction with TC detection | PB/S9.2/L.226 wydanie 4 z dnia 10.04.2024 | |
| 7 | Solid fuels: hard coal, Anthracite, carburiser | Total moisture content Range (0,1 – 40,0) % |
Gravimetric method | PN-ISO 589:2006 Metoda B2 | |
| 8 | Solid fuels: coke | Total moisture content Range (0,1 – 40,0) % |
Gravimetric method | PN-ISO 579:2002 | |
| Mechanical Testing Laboratory Dąbrowa Górnicza; Al. J. Piłsudskiego 92, 41-308 Dąbrowa Górnicza | |||||
| 9 | Steel products | Mechanical properties: proof strength, plastic extension Rp distinct yield strength Re tensile strength Rm elongation A reduction of area Z Range siła F max 600 kN Tensile test at room temperature |
PN-EN ISO 6892-1:2020-05 Metoda B | ASTM A370-22 | ||
| 10 | Steel products | Impact energy Range KV2; KU2 Initial hammer energy 300 J Test temperature: room: 23±5 0C reduced do -50 oC Impact strength test by the Charpy method |
PN-EN ISO 148-1:2017-02 | ||
| 11 | Steel products | HBW hardness Range do 650 HBW Ball diameter 2,5 mm; 10 mm |
Brinell method | PN-EN ISO 6506-1:2014-12 | PN-EN ISO 6506-4:2014-12 | |
| 12 | Steel products | Decarburisation depth Optical microscopy |
Metallographic method | PN-EN ISO 3887:2024:04 | PN-EN 13674-1+A1:2017-07 | |
| 13 | Steel products | Content of nonmetallic inclusions, Optical microscopy | DIN 50602:1985 (metoda K) | PN-EN 13674-1+A1:2017-07 | ||
| 14 | Steel products | Macrostructure, Baumann test | ISO 4968:2022 | PN-EN 13674-1+A1:2017-07 KODEKS UIC 860:2008 | ||
| Mechanical Testing Laboratory - Kraków | |||||
| 15 | Steel products | Mechanical properties distinct yield strength Re proof strength, plastic extension Rp tensile strength Rm elongation A Range siła F max 600 kN Tensile test at room temperature |
PN-EN ISO 6892-1:2020-05 Metoda B | ||
| 16 | Steel products | Impact energy Range KV2 Initial hammer energy 300 J, 450 J Test temperature: room: 23±5 oC reduced do -40 oC Impact strength test by the Charpy method |
PN-EN ISO 148-1:2017-02 | ||
Reference standards (16)
ASTM A370-22
DIN 50602:1985 (metoda K)
ISO 4968:2022
PB/S9.2/L.202 wydanie 3 z dnia 31.03.2022
PB/S9.2/L.203 wydanie 5 z dnia 20.05.2025
PB/S9.2/L.226 wydanie 4 z dnia 10.04.2024
PB/S9.2/L.228 wydanie 4 z dnia 10.03.2026
PN-EN 13674-1+A1:2017-07
PN-EN 13674-1+A1:2017-07 KODEKS UIC 860:2008
PN-EN ISO 148-1:2017-02
PN-EN ISO 3887:2024:04
PN-EN ISO 6506-1:2014-12
PN-EN ISO 6506-4:2014-12
PN-EN ISO 6892-1:2020-05 Metoda B
PN-ISO 579:2002
PN-ISO 589:2006 Metoda B2