🇵🇱 HUTA CZĘSTOCHOWA Sp. z o.o. PL
Materials & polymers
HUTA CZĘSTOCHOWA Sp. z o.o. is a laboratory accredited by PCA under number AB 1038 (Częstochowa, Poland). Its accreditation scope covers 11 test methods in the following areas: Materials & polymers. Test objects include: Metallurgical products, welded joints, Calcium silicon, Fe-Mn, Fe-Cr w/C, nitrided Fe-V, Ferroalloys: Fe-Si, Fe-Mo, Fe-Ti, Fe-B, Fe-V, Fe-Cr n/C, Mn met., F…. Most frequently used techniques: High-temperature combustion with IR detection, Spark excitation atomic emission spectrometry.
At a glance
- Accreditation number: PCA AB 1038
- Methods in scope: 11
- Types of test objects: 10
- Techniques used: 2
- City: Częstochowa, Poland
- Accreditation number
- AB 1038
- Accreditation body
- PCA
- Address
- ul. Kucelińska 22, 42-207 Częstochowa
- City
- Częstochowa, Poland
What this laboratory tests (10)
- Metallurgical products, welded joints — 2 methods
- Calcium silicon — 1 method
- Fe-Mn, Fe-Cr w/C, nitrided Fe-V — 1 method
- Ferroalloys: Fe-Si, Fe-Mo, Fe-Ti, Fe-B, Fe-V, Fe-Cr n/C, Mn met., Fe-P, Fe-Nb, nitrided Fe-Mn, low- and high-alloy steel, steel scrap — 1 method
- Foaming and carburising agent (anthracite-based) carbon-bearing briquette — 1 method
- Graphite electrodes, Foaming agent and carburiser (coke-based) — 1 method
- Pig iron, cast iron, cast iron briquettes, Fe-Si-Mn — 1 method
- Steel — 1 method
- Steelmaking covering powders, Bauxite, Fluxes: lime, dolomitic lime, dolomite, magnesite — 1 method
- Steelmaking dusts — 1 method
Analytical techniques used (2)
- High-temperature combustion with IR detection — 8 methods
- Spark excitation atomic emission spectrometry — 1 method
Laboratory sections (2)
- Chemical and Metallographic Testing Laboratory — 9 methods
- Strength Testing Laboratory — 2 methods
Laboratory locations
- Laboratorium Badań Chemicznych i Metalograficznych — ul. Kucelińska 22, 42-207 Częstochowa
- Laboratorium Badań Wytrzymałościowych — ul. Kucelińska 22, 42-207 Częstochowa
Accreditation scope — test methods (11)
| No. | Test object | Methodology / Parameters | Technique | Reference document | |
|---|---|---|---|---|---|
| Chemical and Metallographic Testing Laboratory | |||||
| 1 | Steel | Content of: C, Mn, Si, P, S, Cu, Cr, Ni, Al, Mo, V, Nb, Sn, As, Ti, N C (0,02 - 1,30) % Mn (0,02 - 1,90) % Si (0,005 - 1,50) % P (0,005 - 0,070) % S (0,002 - 0,070) % Cu (0,01 - 0,60) % Cr (0,01- 3,00) % Ni (0,01 - 2,00) % Al (0,005 - 0,090) % Mo (0,01 - 1,00) % V (0,005 - 0,50) % Nb (0,005 - 0,050) % Sn (0,005 0,10) % As (0,005 - 0,080) % Ti (0,005 - 0,40) % N (0,0020 - 0,0200) % |
Spark excitation atomic emission spectrometry | IL-CH-B-3 Wydanie 1 z dnia 20.12.2024 | |
| 2 | Pig iron, cast iron, cast iron briquettes, Fe-Si-Mn | Carbon and sulphur content C (1,50-4,50) % S (0,010 - 0,20) % |
High-temperature combustion with IR detection | IL-CH-B-1 Wydanie 3 z dnia 24.03.2026 | |
| 3 | Fe-Mn, Fe-Cr w/C, nitrided Fe-V | Carbon and sulphur content C (4,50-8,50) % S (0,010 - 0,10) % |
High-temperature combustion with IR detection | IL-CH-B-1 Wydanie 3 z dnia 24.03.2026 | |
| 4 | Ferroalloys: Fe-Si, Fe-Mo, Fe-Ti, Fe-B, Fe-V, Fe-Cr n/C, Mn met., Fe-P, Fe-Nb, nitrided Fe-Mn, low- and high-alloy steel, steel scrap | Carbon and sulphur content C (0,01 – 1,50) % S (0,0010 - 0,40) % |
High-temperature combustion with IR detection | IL-CH-B-1 Wydanie 3 z dnia 24.03.2026 | |
| 5 | Calcium silicon | Carbon and sulphur content C (0,20 – 0,70) % S (0,010 – 0,035) % |
High-temperature combustion with IR detection | IL-CH-B-1 Wydanie 3 z dnia 24.03.2026 | |
| 6 | Foaming and carburising agent (anthracite-based) carbon-bearing briquette | Carbon and sulphur content C (40,0 - 99,9) % S (0,10 - 1,50) % |
High-temperature combustion with IR detection | IL-CH-B-2 Wydanie 2 z dnia 31.03.2026 | |
| 7 | Graphite electrodes, Foaming agent and carburiser (coke-based) | Carbon and sulphur content C (80,0 - 99,9) % S (0,10 - 1,50) % |
High-temperature combustion with IR detection | IL-CH-B-2 Wydanie 2 z dnia 31.03.2026 | |
| 8 | Steelmaking covering powders, Bauxite, Fluxes: lime, dolomitic lime, dolomite, magnesite | Carbon content Range (0,10 - 30,00) % |
High-temperature combustion with IR detection | IL-CH-B-2 Wydanie 2 z dnia 31.03.2026 | |
| 9 | Steelmaking dusts | Carbon and sulphur content C (0,20 - 6,00) % S (0,20 - 1,50) % |
High-temperature combustion with IR detection | IL-CH-B-2 Wydanie 2 z dnia 31.03.2026 | |
| Strength Testing Laboratory | |||||
| 10 | Metallurgical products, welded joints | Static tensile test at room temperature distinct yield strength Re, proof strength Rp0,2, tensile strength Rm, percentage elongation A5 Force range (3 – 1200) kN |
PN-EN ISO 6892-1:2020-05 Metoda B | ||
| 11 | Metallurgical products, welded joints | Impact strength absorbed impact energy KV2 , KV8 , KU2 , KU8 initial hammer energy 300 J, 450 J test temperature from 20 oC do -60 oC Impact strength test by the Charpy method |
PN-EN ISO 148-1:2017-02 | ||
Reference standards (5)
IL-CH-B-1 Wydanie 3 z dnia 24.03.2026
IL-CH-B-2 Wydanie 2 z dnia 31.03.2026
IL-CH-B-3 Wydanie 1 z dnia 20.12.2024
PN-EN ISO 148-1:2017-02
PN-EN ISO 6892-1:2020-05 Metoda B